IN VITRO SURVIVAL AND FRACTURE FORCE OF LITHIUM DISILICATE HYBRID ABUTMENT CROWNS.
Аннотация
PURPOSE: To evaluate the behavior of hybrid abutment crowns fabricated from monolithic lithium disilicate ceramic (LDC) and to compare the influence of different in vitro artificial aging protocols.
MATERIALS AND
METHODS
A total of 32 monolithic hybrid abutment crowns of monolithic LDC were fabricated. Of these, 24 were artificially aged using three different protocols up to a 20 year simulation (1.2 × 106, 2.4 × 106, 4.8 × 106 chewing cycles, thermocycling), a control group underwent no artificial aging (n = 8, N = 32). Load-to-failure tests were conducted for all specimens, and failure values were compared (P < .05).
RESULTS
All specimens passed in vitro aging. Mean failure load values between 532.6 and 562.8 N were found but did neither differ significantly among the test groups nor from the control group.
CONCLUSIONS
Within the limitations of this in vitro pilot study, hybrid abutment crowns manufactured from monolithic LDC seem to offer appropriate long-lasting mechanical stability over a simulation period up to 20 years. The failure values and complication pattern seem to be independent of several aging protocols in this test set-up.
Предметные рубрики MeSH
Подготовка и перевод публикации
Обработка статьи · этапы, ошибки и управление
Ошибки и ограничения
История · было → стало
Состояние обновляется каждые 5 секунд, пока блок открыт. Процент показывается только там, где известен объём работы. Пауза останавливает продолжение этапа; текущий запрос к источнику может завершиться.
Тип публикации указан по данным источника. Уровень доказательности автоматически не присваивается.