High-Strength and Nonfouling Zwitterionic Triple-Network Hydrogel in Saline Environments.

Li Xiaohui, Tang Chenjue, Liu Di, Yuan Zhefan, Hung Hsiang-Chieh, Luozhong Sijin, Gu Wenchao, Wu Kan, Jiang Shaoyi

СтатьяПеревод в очереди

Аннотация

Zwitterionic hydrogels have received great attention due to their excellent nonfouling and biocompatible properties, but they suffer from weak mechanical strength in the saline environments important for biomedical and engineering applications due to the "anti-polyelectrolyte" effect. Conventional strategies to introduce hydrophobic or non-zwitterionic components to increase mechanical strength compromise their nonfouling properties. Here, a highly effective strategy is reported to achieve both high mechanical strength and excellent nonfouling properties by constructing a pure zwitterionic triple-network (ZTN) hydrogel. The strong electrostatic interaction and network entanglement within the triple-network structure can effectively dissipate energy to toughen the hydrogel and achieve high strength, toughness, and stiffness in saline environments (compressive fracture stress 18.2 ± 1.4 MPa, toughness 1.62 ± 0.03 MJ m-3 , and modulus 0.66 ± 0.03 MPa in seawater environments). Moreover, the ZTN hydrogel is shown to strongly resist the attachment of proteins, bacteria, and cells. The results provide a fundamental understanding to guide the design of tough nonfouling zwitterionic hydrogels for a broad range of applications.

Для цитирования: Li Xiaohui, Tang Chenjue, Liu Di, Yuan Zhefan, Hung Hsiang-Chieh, Luozhong Sijin, Gu Wenchao, Wu Kan, Jiang Shaoyi. High-Strength and Nonfouling Zwitterionic Triple-Network Hydrogel in Saline Environments.. Advanced materials (Deerfield Beach, Fla.). 2021. DOI: 10.1002/adma.202102479.
Подготовка и перевод публикации
Обработка статьи · этапы, ошибки и управление
Загрузка состояния…

История · было → стало

Состояние обновляется каждые 5 секунд, пока блок открыт. Процент показывается только там, где известен объём работы. Пауза останавливает продолжение этапа; текущий запрос к источнику может завершиться.

Тип публикации указан по данным источника. Уровень доказательности автоматически не присваивается.