Fatigue Property and Small Crack Propagation Mechanism of MIG Welding Joint of 6005A-T6 Aluminum Alloy.

Peng Zeng, Yang Shanglei, Wang Zhentao, Gao Zihao

СтатьяПеревод в очереди

Аннотация

In this study, metal inert gas welding (MIG) was applied to 4 mm thick 6005A-T6 aluminum alloy welding. Compared with other parts, the hardness of the weld zone (WZ) was the lowest, about 67 HV. There was the Softening in WZ, which might make WZ the weakest zone. Then, fatigue tests were carried out on MIG welded joints. All the fatigue specimens fractured at the weld toe of the lap joint, and the fracture was characterized by a cleavage fracture. Crack closure induced by oxide was observed during the steady propagation of the fatigue crack. Impurities hindered crack propagation, changed the direction of crack propagation, and appeared in stepped fatigue strip distribution morphology; in the process of the main crack propagation, the initiation and propagation of small cracks were easily restricted and hindered by the main crack, which slowed down the propagation rate and even stopped the propagation directly.

Другие публикации по теме

Для цитирования: Peng Zeng, Yang Shanglei, Wang Zhentao, Gao Zihao. Fatigue Property and Small Crack Propagation Mechanism of MIG Welding Joint of 6005A-T6 Aluminum Alloy.. Materials (Basel, Switzerland). 2022. DOI: 10.3390/ma15134698.
Подготовка и перевод публикации
Обработка статьи · этапы, ошибки и управление
Загрузка состояния…

История · было → стало

Состояние обновляется каждые 5 секунд, пока блок открыт. Процент показывается только там, где известен объём работы. Пауза останавливает продолжение этапа; текущий запрос к источнику может завершиться.

Тип публикации указан по данным источника. Уровень доказательности автоматически не присваивается.