Hydrogel formulations for orthotopic treatment of myocardial infarction.

Luo Qiang, Li Zhibo, Liu Bin, Ding Jianxun

СтатьяОбзорПеревод в очереди

Аннотация

INTRODUCTION

Myocardial infarction (MI) causes extensive structural and functional damage to the cardiac tissue due to the significant loss of cardiomyocytes. Early reperfusion is the standard treatment strategy for acute MI, but it is associated with adverse effects. Additionally, current therapies to alleviate pathological changes post-MI are not effective. Subsequent pathological remodeling of the damaged myocardium often results in heart failure. Oral drugs aimed at reducing myocardial damage and remodeling require repeated administration of high doses to maintain therapeutic levels. This compromises efficacy and patient adherence and may cause adverse effects, such as hypotension and liver and/or kidney dysfunction. Hydrogels have emerged as an effective delivery platform for orthotopic treatment of MI due to their high water content and excellent tissue compatibility.

AREA COVERED: Hydrogels create an optimal microenvironment for delivering drugs, proteins, and cells, preserving their efficacy and increasing their bioavailability. Current research focuses on discovering functional hydrogels for mitigating myocardial damage and regulating repair processes in MI treatment.

EXPERT OPINION: Hydrogels offer a promising approach in enhancing cardiac repair and improving patient outcomes post-MI. Advancements in hydrogel technology are poised to transform MI therapy, paving the way for personalized treatment strategies and enhanced recovery.

Для цитирования: Luo Qiang, Li Zhibo, Liu Bin, Ding Jianxun. Hydrogel formulations for orthotopic treatment of myocardial infarction.. Expert opinion on drug delivery. 2024. DOI: 10.1080/17425247.2024.2409906.

Предметные рубрики MeSH

Подготовка и перевод публикации
Обработка статьи · этапы, ошибки и управление
Загрузка состояния…

История · было → стало

Состояние обновляется каждые 5 секунд, пока блок открыт. Процент показывается только там, где известен объём работы. Пауза останавливает продолжение этапа; текущий запрос к источнику может завершиться.

Тип публикации указан по данным источника. Уровень доказательности автоматически не присваивается.