Аннотация

2-Pyrone-4,6-dicarboxylic acid (PDC) is a chemically stable metabolic intermediate of lignin that can be produced on a large scale by transforming bacteria. Novel biomass-based polymers based on PDC were synthesized by Cu(I)-catalyzed azide-alkyne cycloaddition (CuAAC) and fully characterized by nuclear magnetic resonance, infrared spectroscopies, thermal analysis, and tensile lap shear strength measurements. The onset decomposition temperatures of these PDC-based polymers were all above 200 °C. In addition, the PDC-based polymers exhibited strong adhesive properties to various metal plates, with the highest adhesion to a copper plate of 5.73 MPa. Interestingly, this result was in contrast to our previous findings that PDC-based polymers weakly adhere to copper. Furthermore, when bifunctional alkyne and azide monomers were polymerized in situ under hot-press conditions for 1 h, the resulting PDC-based polymer displayed a similar adhesion to a copper plate of 4.18 MPa. The high affinity of the triazole ring to copper ions improved the adhesive ability and selectivity of the PDC-based polymers to copper while still maintaining the strong adhesive ability to other metals, which is conducive to enhancing the versatility of PDC-based polymers as adhesives.

Для цитирования: Jin Yijie, Joshi Manjusha, Araki Takuma, Kamimura Naofumi, Masai Eiji, Nakamura Masaya, Michinobu Tsuyoshi. Click Synthesis of Triazole Polymers Based on Lignin-Derived Metabolic Intermediate and Their Strong Adhesive Properties to Cu Plate.. Polymers. 2023. DOI: 10.3390/polym15061349.
Подготовка и перевод публикации
Обработка статьи · этапы, ошибки и управление
Загрузка состояния…

История · было → стало

Состояние обновляется каждые 5 секунд, пока блок открыт. Процент показывается только там, где известен объём работы. Пауза останавливает продолжение этапа; текущий запрос к источнику может завершиться.

Тип публикации указан по данным источника. Уровень доказательности автоматически не присваивается.