MedElevator Войти в исследования
← Поиск публикаций

DOI 10.1016/j.carbpol.2017.09.057

Медицинская библиотека · Carbohydrate polymers · 2017

Structural and physicochemical changes in guar gum by alcohol-acid treatment.

Li Dandan, Yang Na, Zhang Yao, Guo Lunan, Sang Shangyuan, Jin Zhengyu, Xu Xueming

СтатьяПеревод в очереди

Аннотация

The aim of this study was to evaluate the effects of alcohol-acid degradation on the structural and physicochemical characteristics of guar gum. Guar gum (50wt.%) was treated with methanol, ethanol, 2-propanol, or 1-butanol containing 1 or 2mL 36% hydrochloric acid at 75°C for 30-240min. The linear relationship between 1/Mw and time suggested that alcohol-acid degradation followed first-order kinetics with rate constants varying directly with the number of alcohol carbon atoms and acid concentration. Alcohol-acid treatment exerted no effect on the chemical and crystal structure of guar but significantly decreased shear viscosity, slightly increased solubility, mildly reduced thermostability, and dramatically darkened colour. This study extended the knowledge of the effect of alcohol on the acid hydrolysis of guar and will contribute to the development of a large-scale procedure for guar gum degradation.

Для цитирования: Li Dandan, Yang Na, Zhang Yao, Guo Lunan, Sang Shangyuan, Jin Zhengyu, Xu Xueming. Structural and physicochemical changes in guar gum by alcohol-acid treatment.. Carbohydrate polymers. 2017. DOI: 10.1016/j.carbpol.2017.09.057.
Подготовка и перевод публикации
Обработка статьи · этапы, ошибки и управление
Загрузка состояния…

История · было → стало

Состояние обновляется каждые 5 секунд, пока блок открыт. Процент показывается только там, где известен объём работы. Пауза останавливает продолжение этапа; текущий запрос к источнику может завершиться.

Тип публикации указан по данным источника. Уровень доказательности автоматически не присваивается.