MedElevator Войти в исследования
← Поиск публикаций

DOI 10.1080/15459620701516162

Медицинская библиотека · Journal of occupational and environmental hygiene · 2007

Particulate and gaseous emissions when welding aluminum alloys.

Cole Homer, Epstein Seymour, Peace Jon

СтатьяПеревод в очереди

Аннотация

Fabrication and repair of aluminum components and structures commonly involves the use of electric arc welding. The interaction of the arc and the metal being welded generates ultraviolet radiation, metallic oxides, fumes, and gases. Aluminum is seldom used as the pure metal but is often alloyed with other metals to improve strength and other physical properties. Therefore, the exact composition of any emissions will depend on the welding process and the particular aluminum alloy being welded. To quantify such emissions, The Aluminum Association sponsored several studies to characterize arc welding emissions by the gas metal arc welding (GMAW) and gas tungsten arc welding (GTAW) processes for various combinations of base and filler alloys. In all cases, the tests were conducted under conditions that could be found in a production weld shop without forced ventilation. The concentrations of each analyte that a welder could be exposed to were greatly affected by the welding process, the composition of the base and filler alloys, the position of the welder, and the welding helmet. The results obtained can be used by employers to identify and control potential hazards associated with the welding of aluminum alloys and can provide the basis for hazard communication to employees involved in the welding of these alloys.

Для цитирования: Cole Homer, Epstein Seymour, Peace Jon. Particulate and gaseous emissions when welding aluminum alloys.. Journal of occupational and environmental hygiene. 2007. DOI: 10.1080/15459620701516162.

Предметные рубрики MeSH

Подготовка и перевод публикации
Обработка статьи · этапы, ошибки и управление
Загрузка состояния…

История · было → стало

Состояние обновляется каждые 5 секунд, пока блок открыт. Процент показывается только там, где известен объём работы. Пауза останавливает продолжение этапа; текущий запрос к источнику может завершиться.

Тип публикации указан по данным источника. Уровень доказательности автоматически не присваивается.