Investigations into the Influence of Temperature on the Tensile Shear Strength of Various Adhesives.
Аннотация
The temperature resistance of glued timber, which is crucial for glued wood construction, represents a significant assessment criterion. To gain insights into this aspect, this study utilized methods such as a shear strength test in accordance with EN 302-1:2013-06 under thermal loading (from 20 °C to 200 °C), and Differential Scanning Calorimetry (DSC) to determine the glass transition temperature (Tg). An increase in thermal load resulted in a decrease in shear strength and an increase in wood breakage. A hierarchy of adhesive groups was established based on strength performance and wood failure percentage (WFP) at 200 °C. Thermoset adhesives (MF: Melamine Formaldehyde, PRF: Phenol Resorcinol Formaldehyde) led the ranking, followed by elastomer adhesives (1C-PUR: One-Component Polyurethane, EPI: Emulsion Polymer Isocyanate), with thermoplastic adhesive (PVAc: Polyvinyl Acetate) last. Thermoset adhesives further cured under heat. PUR adhesives exhibited higher strength performance at 150 °C and lower temperatures.
Подготовка и перевод публикации
Обработка статьи · этапы, ошибки и управление
Ошибки и ограничения
История · было → стало
Состояние обновляется каждые 5 секунд, пока блок открыт. Процент показывается только там, где известен объём работы. Пауза останавливает продолжение этапа; текущий запрос к источнику может завершиться.
Тип публикации указан по данным источника. Уровень доказательности автоматически не присваивается.