In Situ GIWAXS Analysis of Solvent and Additive Effects on PTB7 Thin Film Microstructure Evolution during Spin Coating.
Аннотация
The influence of solvent and processing additives on the pathways and rates of crystalline morphology formation for spin-coated semiconducting PTB7 (poly[[4,8-bis[(2-ethylhexyl)oxy]benzo[1,2-b:4,5-b']dithiophene-2,6-diyl][3-fluoro-2-[(2-ethylhexyl)-carbonyl]-thieno[3,4-b]thiophenediyl]]) thin films is investigated by in situ grazing incidence wide-angle X-ray scattering (GIWAXS) and optical reflectance, to better understand polymer solar cell (PSC) optimization approaches. In situ characterization of PTB7 film formation from chloroform (CF), chlorobenzene (CB), and 1,2-dichlorobenzene (DCB) solutions, as well as CB solutions with 1% and 3% v/v of the processing additives 1-chloronapthalene (CN), diphenylether (DPE), and 1,8-diiodooctane (DIO), reveals multiple crystallization pathways with: (i) single-solvent systems exhibiting rapid (<3 s) crystallization after a solvent boiling point-dependent film thinning transition, (ii) solvent + additive systems exhibiting different crystallization pathways and crystallite formation times from minutes (CN, DPE) to 1.5 h (DIO). Identifying crystalline intermediates has implications for bulk-heterojunction PSC morphology optimization via optimized spin-casting processes.
Подготовка и перевод публикации
Обработка статьи · этапы, ошибки и управление
Ошибки и ограничения
История · было → стало
Состояние обновляется каждые 5 секунд, пока блок открыт. Процент показывается только там, где известен объём работы. Пауза останавливает продолжение этапа; текущий запрос к источнику может завершиться.
Тип публикации указан по данным источника. Уровень доказательности автоматически не присваивается.