Sandwich-Structured PI-FPU/Celgard/PI-FPU Separator for Long-Life Room-Temperature Sodium-Sulfur Batteries.

Jiao Xiaoguang, Yang Chao, Ma Kaixuan, Ge Suyu, Feng Caihong, Jiao Qingze, Zhao Yun

СтатьяПеревод в очереди

Аннотация

The shuttle effect of polysulfides and the piercing of dendrites severely limit the cycling stability and safety of room-temperature sodium-sulfur (RT Na-S) batteries. To address these challenges, a sandwich structure separator was designed and prepared by electrospinning a fluorinated polyurethane copolymerized polyimide (PI-FPU) fiber membrane and assembling it on both sides of a commercial Celgard separator (PI-FPU/Celgard/PI-FPU). The external PI-FPU fiber layers synergistically suppress the polysulfide shuttle through the physical confinement combined with chemical anchoring. Meanwhile, the toughness of the PI-FPU membrane and the high mechanical strength of the Celgard substrate create a robust and flexible structure that effectively inhibits dendrite penetration. In addition, the inherent thermal stability and heat resistance of the PI-FPU material enhance the battery's resistance to thermal runaway and fire. Due to these advanced structural features, the sodium-symmetric cell with the PI-FPU/Celgard/PI-FPU separator achieves stable cycling for over 1000 h at a current density of 1 mA cm-2. The assembled RT Na-S battery maintains a high discharge specific capacity of 555 mAh g-1 after 1500 cycles at 3 A g-1. This work provides a feasible strategy for developing high-safety and long-life RT Na-S batteries.

Для цитирования: Jiao Xiaoguang, Yang Chao, Ma Kaixuan, Ge Suyu, Feng Caihong, Jiao Qingze, Zhao Yun. Sandwich-Structured PI-FPU/Celgard/PI-FPU Separator for Long-Life Room-Temperature Sodium-Sulfur Batteries.. ChemSusChem. 2026. DOI: 10.1002/cssc.202502429.
Подготовка и перевод публикации
Обработка статьи · этапы, ошибки и управление
Загрузка состояния…

История · было → стало

Состояние обновляется каждые 5 секунд, пока блок открыт. Процент показывается только там, где известен объём работы. Пауза останавливает продолжение этапа; текущий запрос к источнику может завершиться.

Тип публикации указан по данным источника. Уровень доказательности автоматически не присваивается.