DOI 10.1111/jopr.70227

Медицинская библиотека · Journal of prosthodontics : official journal of the American College of Prosthodontists · 2026

Fracture resistance of zirconia fixed dental prostheses after low-temperature degradation and/or cyclic fatigue.

Li Yuqi, Zhang Youdong, Lan Yun, Huang Mingming, Wen Jiao, Han Jianmin

СтатьяПеревод в очереди

Аннотация

PURPOSE: Monolithic zirconia fixed dental prostheses (FDPs) are widely used because of their favorable esthetic and mechanical properties. Hydrothermal aging and cyclic fatigue may interact to affect monolithic zirconia FDPs, but evidence from anatomically shaped multi-unit restorations remains limited. This study evaluated fracture resistance, phase transformation, and failure characteristics of three zirconia restorative systems after simulated service exposure.

MATERIALS AND

METHODS

Ninety-six three-unit FDPs were fabricated from self-glazed zirconia (SG), De Corematrix zirconia (DZ), and Lava zirconia (LZ). For each system, the FDPs were divided into four exposure conditions (n = 8): control, cyclic fatigue, low-temperature degradation (LTD), and LTD followed by cyclic fatigue. All specimens were subsequently subjected to load-to-failure testing. Raman spectroscopy and scanning electron microscopy characterized phase transformation and microstructural features.

RESULTS

All cyclically loaded FDPs survived 5 × 106 cycles without macroscopic failure. SG showed the highest control fracture resistance. Cyclic fatigue alone produced little change in SG, whereas LTD and combined exposure markedly reduced its fracture resistance. No exposure-related differences were detected for DZ or LZ, although equivalence was not established. Monoclinic-phase formation was not detected after cyclic fatigue alone but was observed after LTD in all systems and was greater after combined exposure.

CONCLUSIONS

Simulated service exposure affected the zirconia restorative systems differently. SG exhibited the highest initial fracture resistance but was more susceptible to hydrothermal aging. For DZ and LZ, no differences were detected under the present sample size, but stability was not established. All tested FDPs tolerated clinical-level loads, even after long-term service simulations.

Для цитирования: Li Yuqi, Zhang Youdong, Lan Yun, Huang Mingming, Wen Jiao, Han Jianmin. Fracture resistance of zirconia fixed dental prostheses after low-temperature degradation and/or cyclic fatigue.. Journal of prosthodontics : official journal of the American College of Prosthodontists. 2026. DOI: 10.1111/jopr.70227.
Подготовка и перевод публикации
Обработка статьи · этапы, ошибки и управление
Загрузка состояния…

История · было → стало

Состояние обновляется каждые 5 секунд, пока блок открыт. Процент показывается только там, где известен объём работы. Пауза останавливает продолжение этапа; текущий запрос к источнику может завершиться.

Тип публикации указан по данным источника. Уровень доказательности автоматически не присваивается.