Assessment of calcification presence in hydrophilic acrylic phakic intraocular lenses.
Аннотация
PURPOSE: To evaluate explanted hydrophilic acrylic phakic intraocular lenses (pIOLs) for evidence of calcification, specifically the implantable collamer lens (ICL) and the I-CARE.
SETTING
Intermountain Ocular Research Center, John A. Moran Eye Center, University of Utah, Salt Lake City, Utah.
DESIGN
Retrospective laboratory analysis of explanted pIOLs.
METHODS
Demographic data from the explanted cases were collected through a retrospective chart review. Explanted hydrophilic acrylic pIOLs were examined by gross and light microscopy to evaluate optical clarity, material integrity, and presence of surface or subsurface deposits. A subset of lenses underwent histochemical staining (1% alizarin red) and surface analysis to detect calcium deposits. Additional lenses were analyzed with implant cytology and visible-light transmission testing to assess biological deposition and UV-blocking capacity.
RESULTS
84 pIOLs were analyzed, including 65 ICLs (mean implantation time 8.78 ± 7.23 years) and 19 I-CARE lenses (mean implantation time 12.99 ± 5.34 years). Trace to mild pigmentary deposition was present in 36 ICLs (55.4%) and 10 I-CARE lenses (52.6%). No opacification or calcification was observed on gross or microscopic evaluation, including peripheral haptic areas. Histochemical staining and surface analysis confirmed absence of calcium deposits. Implant cytology revealed proteinaceous material without cellular components. Light transmission ranged from 93.7% to 97.4%, and all lenses demonstrated effective UV blocking.
CONCLUSIONS
This large series of explanted hydrophilic acrylic pIOLs showed no evidence of calcification after long-term implantation. These findings support the material stability and biocompatibility of hydrophilic acrylic pIOLs in vivo.
Предметные рубрики MeSH
Подготовка и перевод публикации
Обработка статьи · этапы, ошибки и управление
Ошибки и ограничения
История · было → стало
Состояние обновляется каждые 5 секунд, пока блок открыт. Процент показывается только там, где известен объём работы. Пауза останавливает продолжение этапа; текущий запрос к источнику может завершиться.
Тип публикации указан по данным источника. Уровень доказательности автоматически не присваивается.