BACKGROUND

The minipig has been used for research in various fields of medicine, even in orthopedics. Though previous studies have already suggested other methods to create osteoporotic bone, those methods had some disadvantages for taking time and efforts. Therefore, we aimed to generate osteoporotic proximal humerus and proximal femur of minipig using EDTA solution and validate their properties through dual energy X-ray absorptiometry (DEXA), micro-CT study, histological and biomechanical ways.

METHODS

Six minipigs were used. Out of a total of 12 proximal humerus (PH) and 12 proximal femurs (PF), 6 PH and 6 PF were used as the decalcified group and the opposite side as the non-decalcified group. In vitro decalcification with Ca-chelating agents (0.5 M EDTA solution, pH 7.4) was used. Area BMD (aBMD) was measured using DEXA, Volumetric BMD (vBMD), and microstructure were measured using micro-CT. Universal testing machine was used to measure ultimate load to failure (ULTF). Each group was compared using two types of suture anchors (all-suture anchor, ASA, and conventional screw type anchor, CA).

RESULTS

There was a significant difference in aBMD and cortical thickness (aBMD: decalcified, 0.433 ± 0.073 g/cm2, undecalcified, 0.962 ± 0.123 g/cm2, p < 0.001; cortical thickness: decalcified, 0.33 ± 0.34 mm, undecalcified, 1.61 ± 0.45 mm, p < 0.001). In the case of ASA, the ULTF was significantly lower in the decalcified group (decalcified: 176.6 ± 74.2 N, non-decalcified: 307.7 ± 116.5 N, p = 0.003). In the case of CA, there was no significant difference (decalcified: 265.1 ± 96.0 N, undecalcified: 289.4 ± 114.5 N, p = 0.578).

CONCLUSION

We demonstrated that decalcification with EDTA solution significantly decreased aBMD, vBMD, and cortical thickness. Decalcified minipig bone using EDTA resulted in similar biomechanical properties as osteoporotic human bone with respect to anchor pull-out.

Для цитирования: Seo Jeonghyeon, Kim Hyojune, Min Joongkee, Kim Yongwoo, Jeon In-Ho, D'Lima Darry, Koh Kyoung Hwan. Development of in vitro osteoporosis model in minipig proximal humerus and femur: validation in histological and biomechanical study.. Journal of orthopaedic surgery and research. 2023. DOI: 10.1186/s13018-023-04102-y.

Предметные рубрики MeSH

Подготовка и перевод публикации
Обработка статьи · этапы, ошибки и управление
Загрузка состояния…

История · было → стало

Состояние обновляется каждые 5 секунд, пока блок открыт. Процент показывается только там, где известен объём работы. Пауза останавливает продолжение этапа; текущий запрос к источнику может завершиться.

Тип публикации указан по данным источника. Уровень доказательности автоматически не присваивается.