Functional monomer impurity affects adhesive performance.

Yoshihara Kumiko, Nagaoka Noriyuki, Okihara Takumi, Kuroboshi Manabu, Hayakawa Satoshi, Maruo Yukinori, Nishigawa Goro, De Munck Jan, Yoshida Yasuhiro, Van Meerbeek Bart

СтатьяПоддержка исследования: вне правительства СШАПеревод пока не подготовлен

Аннотация

OBJECTIVE

The functional monomer 10-MDP has been considered as one of the best performing functional monomers for dental adhesives. Different adhesives containing 10-MDP are commercially available, among which many so-called 'universal' adhesives. We hypothesize that the quality of the functional monomer 10-MDP in terms of purity may affect bonding performance.

METHODS

We therefore characterized three different 10-MDP versions (10-MDP_KN provided by Kuraray Noritake; 10-MDP_PCM provided by PCM; 10-MDP_DMI provided by DMI) using NMR, and analyzed their ability to form 10-MDP_Ca salts on dentin using XRD. The 'immediate' and 'aged' micro-tensile bond strength (μTBS) to dentin of three experimental 10-MDP primers was measured. The resultant interfacial adhesive-dentin ultra-structure was characterized using TEM.

RESULTS

NMR disclosed impurities and the presence of 10-MDP dimer in 10-MDP_PCM and 10-MDP_DMI. 10-MDP_PCM and 10-MDP_DMI appeared also sensitive to hydrolysis. 10-MDP_KN, on the contrary, contained less impurities and dimer, and did not undergo hydrolysis. XRD revealed more intense 10-MDP_Ca salt deposition on dentin induced by 10-MDP_KN. The adhesive based on the experimental 10-MDP_KN primer resulted in a significantly higher 'immediate' bond strength that remained stable upon aging; the μTBS of the experimental 10-MDP_PCM and 10-MDP_DMI adhesives significantly dropped upon aging. TEM revealed thicker hybridization and more intense nano-layering for 10-MDP_KN.

SIGNIFICANCE: It was concluded that primer impurities and the presence of 10-MDP dimer affected not only hybridization, but also reduced the formation of 10-MDP_Ca salts and nano-layering. 10-MDP in a high purity grade is essential to achieve durable bonding.

Для цитирования: Yoshihara Kumiko, Nagaoka Noriyuki, Okihara Takumi, Kuroboshi Manabu, Hayakawa Satoshi, Maruo Yukinori, Nishigawa Goro, De Munck Jan, Yoshida Yasuhiro, Van Meerbeek Bart. Functional monomer impurity affects adhesive performance.. Dental materials : official publication of the Academy of Dental Materials. 2015. DOI: 10.1016/j.dental.2015.09.019.

Предметные рубрики MeSH

Подготовка и перевод публикации
Обработка статьи · этапы, ошибки и управление
Загрузка состояния…

История · было → стало

Состояние обновляется каждые 5 секунд, пока блок открыт. Процент показывается только там, где известен объём работы. Пауза останавливает продолжение этапа; текущий запрос к источнику может завершиться.

Тип публикации указан по данным источника. Уровень доказательности автоматически не присваивается.