Construction of metronidazole capped in gold nanoparticles against Helicobacter pylori: antimicrobial activity improvement.
Аннотация
INTRODUCTION
Helicobacter pylori is considered a major agent causing gastritis and peptic ulcer disease. Unfortunately, the occurrence of increasing drug resistance to this bacterium would result in some difficulties in its treatment. Therefore, the application of nanotechnology has been suggested to resolve such problems. Nanoparticles usage in medical research has been expanded in recent years. Among nanometals, gold nanoparticles have exclusive features that can be used in such applications. Using nanotechnology in medical science could help mankind to solve this problem in the future.
AIM: Our aim in this research was to investigate the antimicrobial effect of gold nanoparticles on H. pylori strains.
MATERIALS AND
METHODS
Gold nanoparticles were synthesized by the Turkevich method. Then, their size and dispersion were investigated using spectrophotometry, DLS, and TEM microscopy. Subsequently, the combination of metronidazole and gold nanoparticles was obtained by mixing method, and then the anti-helicobacter effects of the two were evaluated according to CLSI.
RESULTS
The highest size of gold nanoparticles was between 12 and 9 nm, and the maximum absorbance was 522 nm; however, in conjugated state, the maximum absorbance was 540 nm, which indicated the accumulation of drug-conjugated nanoparticles in the conjugate state. Some changes indicated the binding of metronidazole to gold nanoparticles. Antimicrobial testing of gold nanoparticles and metronidazole did not affect the Helicobacter pylori. Therefore, the combination of gold nanoparticles and metronidazole had a 17-mm growth inhibition zone.
CONCLUSIONS
The anti-helicobacter effects of metronidazole significantly increased in conjugation with gold nanoparticles.
Предметные рубрики MeSH
Подготовка и перевод публикации
Обработка статьи · этапы, ошибки и управление
Ошибки и ограничения
История · было → стало
Состояние обновляется каждые 5 секунд, пока блок открыт. Процент показывается только там, где известен объём работы. Пауза останавливает продолжение этапа; текущий запрос к источнику может завершиться.
Тип публикации указан по данным источника. Уровень доказательности автоматически не присваивается.