Experimental maxillary sinus augmentation using a highly bioactive glass ceramic.
СтатьяПоддержка исследования: вне правительства СШАНазвание и аннотация: Перевод пока не подготовлен
Обработка статьи · этапы, ошибки и управление
Загрузка состояния…
Ошибки и ограничения
История · было → стало
Состояние обновляется каждые 5 секунд, пока блок открыт. Процент показывается только там, где известен объём работы. Пауза останавливает продолжение этапа; текущий запрос к источнику может завершиться.
Vivan Rodrigo Ricci, Mecca Carlos Eduardo, Biguetti Claudia Cristina, Rennó Ana Claudia Muniz, Okamoto Roberta, Cavenago Bruno Cavalini, Duarte Marco Húngaro, Matsumoto Mariza Akemi
Аннотация
Physicochemical characteristics of a biomaterial directly influence its biological behavior and fate. However, anatomical and physiological particularities of the recipient site also seem to contribute with this process. The present study aimed to evaluate bone healing of maxillary sinus augmentation using a novel bioactive glass ceramic in comparison with a bovine hydroxyapatite. Bilateral sinus augmentation was performed in adult male rabbits, divided into 4 groups according to the biomaterial used: BO-particulate bovine HA Bio-Oss(®) (BO), BO+G-particulate bovine HA + particulate autogenous bone graft (G), BS-particulate glass ceramic (180-212 μm) Biosilicate(®) (BS), and BS+G-particulate glass ceramic + G. After 45 and 90 days, animals were euthanized and the specimens prepared to be analyzed under light and polarized microscopy, immunohistochemistry, scanning electron microscopy (SEM), and micro-computed tomography (μCT). Results revealed different degradation pattern between both biomaterials, despite the association with bone graft. BS caused a more intense chronic inflammation with foreign body reaction, which led to a difficulty in bone formation. Besides this evidence, SEM and μCT confirmed direct contact between newly formed bone and biomaterial, along with osteopontin and osteocalcin immunolabeling. Bone matrix mineralization was late in BS group but became similar to BO at day 90. These results clearly indicate that further studies about Biosilicate(®) are necessary to identify the factors that resulted in an unfavorable healing response when used in maxillary sinus augmentation.