DOI 10.1016/j.joca.2008.05.020
Inorganic pyrophosphate as a regulator of hydroxyapatite or calcium pyrophosphate dihydrate mineral deposition by matrix vesicles.
Аннотация
OBJECTIVE
Pathological mineralization is induced by unbalance between pro- and anti-mineralization factors. In calcifying osteoarthritic joints, articular chondrocytes undergo terminal differentiation similar to that in growth plate cartilage and release matrix vesicles (MVs) responsible for hydroxyapatite (HA) or calcium pyrophosphate dihydrate (CPPD) deposition. Inorganic pyrophosphate (PP(i)) is a likely source of inorganic phosphate (P(i)) to sustain HA formation when hydrolyzed but also a potent inhibitor preventing apatite mineral deposition and growth. Moreover, an excess of PP(i) can lead to CPPD formation, a marker of pathological calcification in osteoarthritic joints. It was suggested that the P(i)/PP(i) ratio during biomineralization is a turning point between physiological and pathological mineralization. The aim of this work was to determine the conditions favoring either HA or CPPD formation initiated by MVs.
METHODS
MVs were isolated from 17-day-old chicken embryo growth plate cartilages and subjected to mineralization in the presence of various P(i)/PP(i) ratios. The mineralization kinetics and the chemical composition of minerals were determined, respectively, by light scattering and infrared spectroscopy.
RESULTS
The formation of HA is optimal when the P(i)/PP(i) molar ratio is above 140, but is completely inhibited when the ratio decreases below 70. The retardation of any mineral formation is maximal at P(i)/PP(i) ratio around 30. CPPD is exclusively produced by MVs when the ratio is below 6, but it is inhibited for the ratio exceeding 25.
CONCLUSIONS
Our findings are consistent with the P(i)/PP(i) ratio being a determinant factor leading to pathological mineralization or its inhibition.
Предметные рубрики MeSH
Подготовка и перевод публикации
Обработка статьи · этапы, ошибки и управление
Ошибки и ограничения
История · было → стало
Состояние обновляется каждые 5 секунд, пока блок открыт. Процент показывается только там, где известен объём работы. Пауза останавливает продолжение этапа; текущий запрос к источнику может завершиться.
Тип публикации указан по данным источника. Уровень доказательности автоматически не присваивается.