Rapid corrosion and the absence of non-invasive readouts limit the clinical translation of biodegradable magnesium implants. Here, AZ31 magnesium alloy was alkali-treated and coated with chitosan (AZ31-CS) or a chitosan/upconversion nanoparticle composite (AZ31-CN; NaYF₄:Yb3⁺,Er3⁺ ) to couple corrosion control with fluorescence-guided degradation tracking. In simulated body fluid, chitosan-based coatings reduced corrosion rate, pH increase, and hydrogen evolution compared with AZ31-OH. For AZ31-CN, near-infrared excitation generated visible emission, and fluorescence intensity decreased during immersion, serving as a surrogate indicator of coating degradation. MC3T3-E1 assays demonstrated good cytocompatibility, enhanced proliferation, and increased osteogenic differentiation, evidenced by elevated ALP activity, mineralization, and upregulated ALP, OPN, and RunX2 expression. In a rat calvarial defect model, coated samples showed higher bone volume fraction and trabecular number than AZ31-OH. The chitosan/UCNPs coating provides a multifunctional biointerface integrating degradation regulation with optical monitoring for traceable magnesium-based bone implants.

Для цитирования: Sun Ming, Sun Danfang, Yin Xiumei, Wang Yanfu, Shi Zheng, Chen Jianduo, Xiong Guokai, Zhang Yunshuo, Wang Chengyue. Fluorescence-trackable chitosan/UCNPs coatings regulate magnesium alloy corrosion and osteogenesis.. Colloids and surfaces. B, Biointerfaces. 2026. DOI: 10.1016/j.colsurfb.2026.115939.

Предметные рубрики MeSH

Подготовка и перевод публикации
Обработка статьи · этапы, ошибки и управление
Загрузка состояния…

История · было → стало

Состояние обновляется каждые 5 секунд, пока блок открыт. Процент показывается только там, где известен объём работы. Пауза останавливает продолжение этапа; текущий запрос к источнику может завершиться.

Тип публикации указан по данным источника. Уровень доказательности автоматически не присваивается.